TABLA 3: AISLAMIENTO TÉRMICO CON CONCRETO AIREADO LITEBUILT®
Goldbar
Densidad de Concreto
kg/m³
λ
Valor de Resistencia

100mm

K a Espesores Determinados de Concreto
50mm
100mm
150mm
200mm
300
0.065
1.54
1.03 0.58 0.40 0.30
400
0.080
1.25
1.21
0.69
0.46
0.37
500
0.095
1.05
1.38
0.80
0.56
0.43
600
0.115
0.87
1.57
0.93
0.67
0.52
700
0.130
0.76
1.23
0.89
0.63
0.47
800
0.150
0.66
1.37
1.00
0.71
0.54
900
0.175
0.57
1.52
1.13
0.81
0.61
1000
0.205
0.48
1.69
1.27
0.94
0.70
1100
0.230
0.43
1.82
1.39
1.02
0.78
1200
0.270
0.37
2.02
1.55
1.15
0.98
1400
0.346
0.43
2.31
1.83
1.39
1.08
1600
0.436
0.28
2.06
2.10
1.63
1.29

  λ = Coeficiente de Conductividad Térmica
K = Coeficiente de Transmisión Térmica

Nota: Las densidades de 300-600 son mezclas de cemento/espuma solamente
Las densidades de 700 y más son mezclas de cemento/arena/espuma